I think you need to really test this in the sun. I made some PLA parts and left them in my trunk of my Model 3 for a few days and the heat caused them to deform a lot. I've noticed my CT panels get super hot when sitting in the sun. You may have to consider a more heat resistant filament. I was...
Why don't you include the denatured alcohol? Seems like you tried to add everything you need EXCEPT that. Even when you specify a specific type of denatured alcohol. Would be nice if it truly was a COMPLETE kit and not having to run to the hardware store on top.
I assume there has to be quite a "preparation" too to get the stainless as clean and perfect as possible before you seal it. Just like for Clear PPF. You don't want to seal in an inconsistent stainless look.
May have to do the Beekeper's Friend polishing to get all the panels as perfect as...